Influence Factors on Magnetic Induction of Traveling Wave Electromagnetic Stirrer for Slab Concasting
Xing Shuqing, Ma Yonglin, Su Guodong, Huang Haie, Li Jianchao
Special Steel . 2006, (3): 20 -22 .