Practice of GCr15 Bearing Steel Production by 50 t EBT  EAF-LF(VD)-  CC  Process
Li Faxing, Lan Xinzhe, Song Yonghui, Hu Mengjun, Sun Yongxi
Special Steel . 2006, (3): 57 -58 .