ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Process Practice of GCr15 Bearing Steel With 60 t Consteel EAF-LF(VD)- CC Flow Sheet at Guiyang Steel
Xia Huihua, Wang Xiang, Yuan Renping , Zhou Yinghao
Special Steel . 2006, (3): 59 -60 .