ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Control and Analysis on Edge Crack of Hot Rolled Strip Coil Produced by CSP Process
Sun Yanhui, Zhao Changliang, Meng Zhengbing, Cai Kaike, Cheng Xiaojun, Wu Guangliang, Zhou Chunquan⊃2;
Special Steel . 2006, (4): 47 -49 .