Temperature Prediction of GCr15 Biilet Core Based on Heating Furnace Embedded Thermocouple Experiment
Han Huaibin , Yu Xueqing , Bai Ruijuan , Wang Wei , Wu Siwei , Zhao Xianming
Special Steel . 2023, (2): 1 -6 .  DOI: 10.20057/j.1003-8620.2022-00126