Development of Mold Flux for Continuous Casting of Cr13 Type Martensitic Stainless Steel Square Billet
Feng Weimin, Xue Jingheng, Xing Guocheng, Ren Fei, Wang Hongpo, Wang Yu
Special Steel . 2023, (3): 53 -58 .  DOI: 10.20057/j.1003-8620.2022-00220