Development of High Strengthening and Toughening TMCP of 40MnVS Steel Round Bars for Direct Cutting Appliction
Ji Ling , Yu Daojun
Special Steel . 2023, (2): 25 -28 .  DOI: 10.20057/j.1003-8620.2022-00016