ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Bubble Analysis of Macrostructure of WB36 Thick Wall Seamless Steel Pipe and Process Research
Xia Yunfeng , Zhou Zhongcheng , Hu Yongping , Lin Yu
Special Steel . 2023, (2): 29 -32 .  DOI: 10.20057/j.1003-8620.2022-00127