ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Development of Hot-Rolled Wire Rods of 35CrMo Annealing-Free Cold Heading Steel for High-Strength Bolts
Wang Haihua , Zheng Xiaowei , Zhang Jianfeng , Lin Zaiyong , Kong Xiangwei
Special Steel . 2023, (2): 33 -36 .  DOI: 10.20057/j.1003-8620.2022-00075