Production Practice of Duplex Stainless Steel Wire Rods ER2209 for Welding Application
Li Li , Ji Dengping , Ma Zhenyu , Yan Daocong , Hu Meiqing , Wang Zhenying , Xie Dongxi
Special Steel . 2023, (2): 37 -42 .  DOI: 10.20057/j.1003-8620.2022-00005