ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Cooling Rate on Mechanical Properties and Microstructure of New C61 Gear Steel
Qi Ming , Liang Xiaodong , Han Dahong , Ren Jianmin , Zhang Zhichao , Wang Xu
Special Steel . 2023, (2): 80 -83 .  DOI: 10.20057/j.1003-8620.2022-00106