A Study of Water Model on Mixing Characteristics of Powder Injected through Top Lance in RH-PTB Vacuum Refining Unit
Du Chengwu , Zhu Miaoyong , Pan Shisong , Zheng Shuguo
Special Steel . 2005, (5): 16 -18 .