Thermodynamic Calculation and Analysis on Equilibrium Phases Transition in T122 Heat-Resistant Steel
Cao Jinrong, Liu Zhengdong , Cheng Shichang, Yang Gang, Xie Jianxin
Special Steel . 2005, (6): 16 -17 .