Process Practice of Tap-to-Tap Time Controlling for an 100 t AC Shaft Arc Furnace at Anyang Steel
Zhang Dianjun, Liang Shiyong, Song Wanping, Du Yong
Special Steel . 2005, (6): 50 -51 .