Development of V Microalloy HSLA Steel Produced by Thin Slab Casting and Rolling Process
Mao Xinping, Li Chunyan, Liu Qingyou, Lin Zhenyuan, Zhuang Hanzhou, Cao Jixiang
Special Steel . 2006, (5): 51 -52 .