ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Research and Development of Single Weight 50 t  Grade 174 mm 12Cr2MolR ( H) Steel Plate
Hou Jingchao, Zhao Guochang, Li Jie, Long Jie, Wu Yanyang, Yuan Jincheng
Special Steel . 2022, (1): 57 -61 .