Study On 350 ℃ High Temperature Mechanical Properties of High Strength TP110H Thermal Production Well Casing Pipe
Wu Liangliang, Wu Yongchao, Zhou Jiaxiang, Zhang Xu
Special Steel . 2023, (4): 125 -128 .  DOI: 10.20057/j.1003-8620.2022-00194