A Study on Dynamic Recrystallization of a Nb- Bearing Low Carbon Steel Q345C during CSP Rolling
He Jianzhong, Liu Yazhen, Shi Liu , Liu Qingyou, Wang Xuelian, Li Degang
Special Steel . 2005, (3): 9 -11 .