Pilot Production of Forged Semi- High Speed Steel Working Roll for Cold Rolling
Yin Zhongda , Liu Defu, Xu Dexiang, Li Zhaohua, Sun Xuele , Gao Feng
Special Steel . 2005, (4): 38 -39 .