Thermodynamic Analysis of the Phase Transition of Supper Austenitic Stainless Steel S31254
Zhang Wei, Wang Qi, Wang Lijun, Li Jianmin
Special Steel . 2023, (4): 8 -14 .  DOI: 10.20057/j.1003-8620.2022-00232