Physical and Mathematical Simulation on Flow Control Devices of Tundish for Thin Slab Concaster
Xue Weifeng, Wen Guanghua, Tang Ping, Song Chao, Sheng Chang, Huang Sheqing, Shi Xiangying, Pan Yuanwang
Special Steel . 2005, (3): 19 -21 .