ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Influence of Work Hardening on Railway Frog Surface Spalling of 1.14C-12.72Mn High Manganese Steel
Zhang Min, Wang Weibo, Zhou Yongxin, Lu Zhenlin, An Qiang
Special Steel . 2005, (3): 45 -47 .