Effect of Heat Treatment on Microstructure and Properties of Brake Disc for High-Speed Trains with 350 km/h
Li Kaixin, Deng Wei, Wen Hui, Yu Liangji, Wu Dongsheng, Wang Fuming
Special Steel . 2023, (4): 80 -87 .  DOI: 10.20057/j.1003-8620.2022-00228