Effect of AlN and Zr Microalloying on Thermoplasticity and Grain Size of Carburized Gear Steel
Yang Feifei, Xu Haiwei, Gen Hao, Ji Chenxi, Di Guobiao
Special Steel . 2023, (4): 94 -101 .  DOI: 10.20057/j.1003-8620.2023-00020