Optimization and Industrial Application of 210 t Converter Oxygen Lance Jet-Flow Performance
Yang Dongya, Peng Qichun, Tong Zhibo, Liu Hongjun, Wu Pinghui, Tan Dajin, Xie Cheng
Special Steel . 2023, (4): 15 -21 .  DOI: 10.20057/j.1003-8620.2023-00027