Development of Adding Bi-Ce Free-Cutting Stainless  Steel 1.4104 for Electro-hydraulic Controller
Lei Yinghua, Liu Shangtan, Zhang Jun, Zheng Zhenyu, Liao Kai
Special Steel . 2022, (1): 73 -77 .