Study on Strength and Toughness of Nb-Ti Microalloying X65MO Deep Sea Pipeline Steel Plate and Steel Tube
Fang Lei , Zuo Xiurong, Jiang Jinxing , Liu Shuai and Zhai Dongyu
Special Steel . 2021, (1): 86 -90 .