Thermodynamic Simulation of GH3128 Alloy Based on CALPHAD Method and Application
Liu Tingyao, Zhang Jian, Lai Yu, Wei Yujun, He Yunhua , Pei Binghong
Special Steel . 2020, (1): 1 -5 .