AOD Nitrogen Control Pratice of of Low Carbon 400 Series Ferritic Stainless Steel at Xingtai Iron and Steel
Li Guangbin, Zhao Yingkai, Wu Guanghai, Yang Qiangqiang , MuYongwei, , Guo Zhibin
Special Steel . 2020, (1): 24 -27 .