Effect of Solution Temperature on Impact Property of New Co-free Maraging Steel 00Nil4Cr3Mo3Ti
Ren Yanni , Liu Zhouli, Yang Weiyu , Zhao Weidong
Special Steel . 2020, (1): 64 -67 .