Water Model Experiment on Interaction Between Innovated Double-Structure Oxygen Lance and Converter Molten Pool
Zhang Guoxin, Liu Guangqiang, Liu Kun , Li Huixiang
Special Steel . 2020, (2): 6 -9 .