Practice and Analysis of Light Calcium Treatment of 55Cr3 Aluminum Deoxidized Spring Steel
Li Xue, Wu Huajie, Liu Wei, Sun Yanhui, Li Ming
Special Steel . 2023, (4): 49 -53 .  DOI: 10.20057/j.1003-8620.2023-00038