Effect of Quenching Cooling Method on Low-temperature Impact Toughness of 20Cr1Mo1VTiB High Temperature Bolting Steel
Gong Xueting, Zhao Jiqing, Yang Gang, Yang Bin
Special Steel . 2023, (4): 88 -93 .  DOI: 10.20057/j.1003-8620.2023-00006