The Effect of Electroslag Remelting Slag System on Inclusions in C-HRA-3 Heat-Resistant Alloy
Li Longfei, Lin Tengchang, Zhang Qiang, He Xikou, Chen Zhengzong , Zhou Xiaozhou
Special Steel . 2023, (5): 76 -82 .  DOI: 10.20057/j.1003-8620.2023-00089