The Influence on Micro-defect of Hydrogen in Middle Carbon Bearing Steel C56E2
Chen De, Liu Jigang, Zhou Yang
Special Steel . 2023, (6): 117 -122 .  DOI: 10.20057/j.1003-8620.2022-00247