Research and Development of YL82B-QM High-strength Steel Strand by On-line Heat Treatment Technology
Yan Chaonan, Xu Kai, Zhang Wentao, Chen Dianqing, Yuan Xiangkun, Li Maimai
Special Steel . 2023, (5): 43 -46 .  DOI: 10.20057/j.1003-8620.2023-00083