ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Verification and Application of Austenite Grain Growth Model in 34CrNi3MoV Steel
Zheng Bing, Xu Dong, Wang Yiqun, Wang Xuexi, Zhao Hongyang, Ju Dongying
Special Steel . 2023, (6): 101 -106 .  DOI: 10.20057/j.1003-8620.2023-00024