Optimization and Simulation of Stirring Process for 100 t Electric Arc Furnace Bath and Its Application
Zeng Zhaopeng, Du Xiqian, Wang Yao, Ma Jianchao
Special Steel . 2023, (6): 45 -52 .  DOI: 10.20057/j.1003-8620.2023-00051