Thermodynamic Simulation of Equilibrium Solidification and Precipitation of CW12MW and CW6MC Cast Nickel-based Alloys
Su Xue hu
Special Steel . 2023, (6): 31 -38 .  DOI: 10.20057/j.1003-8620.2023-00063