ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

The Smelting Process Improvement of 120 t Top-Bottom Combined Blown Converter with High-Carbon Turndown and Low Phosphorus Tapping
Zhang Fudong, Wu Bo, Wang Yuecong, Zhao Xin, Liang Chao
Special Steel . 2023, (6): 63 -69 .  DOI: 10.20057/j.1003-8620.2023-00049