Numerical simulation and Process Practice of Mold Electromagnetic Stirring for IF Steel Slab
Liu Qilong, Deng Yong, Li Huagang, Wei Rujun, Cao Chenghu, Zhang Min
Special Steel . 2023, (6): 83 -88 .  DOI: 10.20057/j.1003-8620.2023-00119