Effect of Tundish Coating on Cleanliness of GCr15 Bearing Steel
Jiang Yaqing, Chen Jun, Huang Chenggang, Li Bo, Li Qian, Jiang Yanfeng
Special Steel . 2024, (1): 61 -64 .  DOI: 10.20057/j.1003-8620.2022-00178