Fracture Analysis of Toughness Fracture Failure on Flexspline of Harmonic Reducers During the Service
Mu Xiaobiao, Zhang Yongqi, Gao Minyan, Yang Guoqiang, Zhang Chaolei
Special Steel . 2024, (1): 98 -102 .  DOI: 10.20057/j.1003-8620.2023-00118