Steelmaking Production Practice of 9Ni Steel for Ulta-low Temperature Pressure Vessel
Zhang Tianshu, Huang Zhicheng, Chi Yunguang, Yang Jian
Special Steel . 2024, (1): 27 -32 .  DOI: 10.20057/j.1003-8620.2023-00174