Practice of Economical Smelting of Q355 Steel in Converter
Huang Gaojian, Wei Zehong, Song Huan, Zhan Dongping, Geng Bin, Yang Yongkun
Special Steel . 2024, (1): 70 -76 .  DOI: 10.20057/j.1003-8620.2023-00203