Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish
Li Jingshe, Wang Cun, Chen Yongfeng, Yang Shufeng, Liu Wei, Bai Yun, Huang Chengyong, Sun Ye
Special Steel . 2024, (1): 1 -11 .  DOI: 10.20057/j.1003-8620.2023-00239