Influence of Sulfur Content on Inclusion and Fatigue Properties of 18CrNiMo7-6 Gear Steels
Yu Wenchao, Xie Dirong, Shi Jie, Wang Maoqiu
Special Steel . 2024, (1): 111 -116 .  DOI: 10.20057/j.1003-8620.2023-00091