Research on a Steel Leakage Prediction Model Based on One vs Rest Genetic Algorithm Optimization Decision Tree
Yu Haochen, Zhang Benguo, Wu Heng, Zhang Ruizhong
Special Steel . 2024, (2): 112 -117 .  DOI: 10.20057/j.1003-8620.2023-00245