Development of Rolled Steel Products from 3 t Ingot of Grade 8620 for Railway Axle Box Bearings
Li Bopeng , Tao Shijun, Zhang Jianfeng, Liu Yueyun, Lu Zhujun, Lv Wenjun
Special Steel . 2024, (3): 1 -4 .  DOI: 10.20057/j.1003-8620.2023-00011