Research and Development of 10B38 Boron Containing Cold Heading Steel
Ma Liguo, Guo Dayong, Wang Bingxi, Gao Hang , Zhang Bo, Pan Yang
Special Steel . 2024, (3): 10 -14 .  DOI: 10.20057/j.1003-8620.2023-00210